Danyang City Kaixin Alloy Material Co., Ltd.

Kovar wire

Kovar wire
Product Detailed

kovar wire specification:0.20-8mm.
Cold drawn state,soft or hardness.
bright and shining
coil packing
Major manufacturers

Note:1.Alloy grades and chemical composition consistent with the provisions of table 1

the chemical composition of Kovar(%)

C

P

S

Mn

Si

Cu

Cr

Mo

Ni

Co

   Fe

         Not more than≤

 

 

 

0.03

0.020

0.020

0.5

0.30

0.20

0.20

0.20

28.5~29.5

16.8~17.8

balance

 

2.The tensile strength of wire in line with the provisions of Table 2

Status code

State

Tensile strength,N/mm2

R

1/4I

1/2I

3/4I

I

Soft state

1/4 Hard state

1/2 Hard state

3/4 Hard state

Hard state

<585

585-725

655-795

725-860

>860

 

3.Strip tensile strength in line with the provisions of Table 3

Status code

State

Tensile strength,N/mm2

R

1/4I

1/2I

3/4I

I

Soft state

1/4 Hard state

1/2 Hard state

3/4 Hard state

Hard state

<570

520-630

590-700

600-770

>700

 

4.Alloy average linear expansion coefficient in line with the Table 4                  

Alloy Grades

Specimen heat treatment system

The average linear expansion coefficient a,10-6/ oC

20-

300oC

20-

400oC

20-

450oC

 

kovar

In hydrogen atmosphere heated to 900 ± 20 oC, insulation 1h, and then heated to 1100 ± 20 oC, insulation 15min, to not more than 5 oC / min rate of cooling to below 200 oC released.

 

-----

 

4.6-5.2

 

5.1-5.5

 

 

 

 

 

 

 

 

5.Alloy typical expansion coefficient                                                 

Alloy Grades

 

The average linear expansion coefficient a,10-6/ oC

20-200oC

20-300oC

20-400oC

20-450oC

20-500oC

20-600oC

20-700oC

20-800oC

kovar

5.9

5.3

5.1

5.3

6.2

7.8

9.2

10.2

                                                                               



Copyright Notice @ 2008-2022 B2BAGE Limited and/or its subsidiaries and licensors. All rights reserved.